Grand Forks Mobile Welding

Farm equipment repair: what welds and what doesn't

Some broken parts are a twenty-minute weld. Some take a slow, careful procedure. A few should never see an arc. Here is how to tell them apart.

Start by knowing what the metal is

Most farm machinery is mild steel, and mild steel welds well. The trouble comes from the parts that aren't: cast housings and brackets, hardened wear parts, and coated metal. The same crack can be a routine repair in one material and a lost cause in another, so the first question a welder asks is "what is it made of?"

Clues you can check before you call:

Tell the welder what you found, and text a photo of the break if you can.

Cast iron: possible, but slow and fussy

Lincoln Electric's guidance calls cast iron "difficult, but not impossible" to weld. The reason is carbon: cast iron typically carries 2 to 4 percent carbon, roughly ten times as much as most steels. Castings are made by letting molten iron cool slowly, and a weld repair has to respect that. Lincoln's rule is that during and after welding, the casting must either cool slowly or be kept cool enough that the cooling rate doesn't matter.

That gives two workable methods, and Lincoln says to pick one and stick with it:

Lincoln adds that nickel-type electrodes are needed if the part will be machined afterward, and that tiny cracks next to the weld are common in cast iron even with good procedure, which matters if the part has to hold oil or water.

Brazing is another route. Miller notes that silicon bronze can braze dissimilar metals including cast iron, at lower heat than welding, but also warns that brazed joints should not be used where structural integrity is needed. A brazed cover or a non-load-bearing bracket can be fine. A cracked axle housing is a different conversation.

High-carbon and hardened steel

Not all steel is mild steel. Miller's equipment-repair guidance says preheating is typically required on all thicknesses once the carbon content of the steel goes above 0.40 percent, and recommends an oxy-fuel torch with a rosebud tip plus temperature-indicating crayons to check it. Miller's advice when you don't know the exact grade is to ask the material supplier.

TWI, the UK welding research institute, explains why: hydrogen cracking needs three things together, hydrogen from the welding process, a hard and brittle structure in the steel, and tensile stress. Higher-carbon and alloy steels form that hard structure easily. For steels with a carbon equivalent above about 0.5, TWI lists preheat, low-hydrogen welding, post-weld heating and slow cooling as the usual precautions.

In farm terms, that covers a lot of the parts that wear: cutting edges, some shanks and points, hardened pins, springs. Ask the manufacturer or dealer before welding anything sold as heat-treated or wear-resistant. Sometimes the right answer is a new part, and hardfacing the new one.

Never weld these

Wheels and rims. OSHA's rule for servicing large-vehicle wheels says cracked, broken, bent or otherwise damaged rim components shall not be reworked, welded, brazed or otherwise heated, and that no heat shall be applied to a multi-piece wheel or a single-piece wheel. That rule is written for workplaces that service truck and equipment wheels (it does not cover car and light-truck wheels, and farm work falls under OSHA's separate agriculture standards instead), but the reasoning applies anywhere: a mounted tire holds a lot of stored energy, and heat on the rim is how wheels come apart. Replace damaged wheels.

Rollover protective structures (ROPS). The Central States Center for Agricultural Safety and Health at the University of Nebraska Medical Center is blunt: never drill holes into a ROPS frame or weld additional steel to it. Clamp lights and accessories on instead. A ROPS is engineered and tested for a specific tractor, and after a tractor rolls, the ROPS must be replaced because it is designed to absorb a single overturn. The same source says homemade ROPS are not recommended, that dealers can install retrofit ROPS and seat belts, and that the University of Kentucky keeps a searchable guide to ROPS for many tractor models.

Paint, galvanizing and grease

OSHA's fact sheet on welding fume says welding surfaces should be cleaned of coatings that could create toxic exposure, such as paint and solvent residue. Zinc, the coating on galvanized steel, is one of the metals OSHA lists in welding fume, and metal fume fever is among the health effects it names. Outdoors, OSHA's advice is to stay upwind.

Cleaning matters for the weld itself too. Miller says rust, oil and paint must be ground or wiped away before welding, or the result is a failed or weakened weld. If you have a few minutes before the welder arrives, scrape off caked dirt and grease around the break. Don't grind a crack open yourself unless the welder asks you to.

What to have ready for the call

The welder may tell you a part should be replaced rather than repaired. On wheels, rollover frames, and some cast and hardened parts, that is the honest answer.